  • Hot wear resistance 40%
  • Plastic deformation resistance 40%
  • Heat checking resistance 40%
  • Premature cracking resistance 35%

Reference steel AISI H13

  • Hot wear resistance 40%
  • Plastic deformation resistance 40%
  • Heat checking resistance 40%
  • Premature cracking resistance 35%

Chemical composition

C Si Mn Cr Mo V
0.39 1.00 0.40 5.30 1.30 0.90