  • Hot wear resistance 90%
  • Plastic deformation resistance 80%
  • Heat checking resistance 30%
  • Premature cracking resistance 15%

Reference Grade Hot Work (H13)

  • Hot wear resistance 40%
  • Plastic deformation resistance 40%
  • Heat checking resistance 40%
  • Premature cracking resistance 35%

Designations

Chemical composition

C Si Mn Cr Mo V
0.70 0.20 0.45 5.00 2.25 1.60